Advanced atomic layer deposition enables lithium-ion battery technology

11-May-2017 - USA

The U.S. Department of Energy's National renewable energy Laboratory (NREL) has entered into an exclusive license agreement with Forge Nano to commercialize NREL's patented battery materials and systems capable of operating safely in high-stress environments. A particular feature of the technology is the encapsulation of materials with solid electrolyte coatings that can be designed to meet the increasingly demanding needs of any battery application.

These lithium-ion batteries feature a hybrid solid-liquid electrolyte system, in which the electrodes are coated with a solid electrolyte layer. This layer minimizes the potential for the formation of an internal short circuit between electrodes to prevent "thermal runaway," or the uncontrolled increase in battery cell temperature that can result in a fire or an explosion.

In addition, coating of the electrode materials reduces the stress on traditional polymer separators that are currently necessary components in commercial lithium-ion batteries and can allow for thinner separators designed for higher power devices. This advancement has the potential to reduce both the cost and weight of the battery device, while substantially increasing safety and lifetime.

Lab-scale testing of NREL's hybrid solid-liquid electrolyte system has shown increased electrode durability and reliability without compromised electrochemical performance. "The cells are less likely to fail, even in demanding, real-world conditions like high temperatures and fast recycle rates," said Ahmad Pesaran, whose team of engineers in NREL's Energy Storage group invented the technology.

Forge Nano, formerly PneumatiCoat Technologies, is a Colorado-based company specializing in the scale-up and manufacturing of cost-effective Atomic Layer Deposition (ALD) encapsulated materials. Forge Nano presented its technology at the 2013 and 2017 NREL Industry Growth Forum, the nation's premier clean energy investment event. A year later, NREL approached the company as a potential licensee after conducting a licensee search in the battery technology area.

"This license agreement will allow Forge Nano to offer further customized lithium-ion battery materials for high performance devices by utilizing our patented high-throughput ALD system that has already been successfully tested at the pilot scale and in large format pouch cells," Paul Lichty, CEO of Forge Nano, said. "The incorporation of this technology into Forge Nano's offering will lead to a substantial reduction in cost per unit energy of lithium-ion batteries."

Other news from the department science

These products might interest you

OCA 200

OCA 200 by DataPhysics

Using contact angle meter to comprehensively characterise wetting behaviour, solids, and liquids

With its intuitive software and as a modular system, the OCA 200 answers to all customers’ needs

contact angle measuring instruments
Tailor-made products for specific applications

Tailor-made products for specific applications by IPC Process Center

Granulates and pellets - we develop and manufacture the perfect solution for you

Agglomeration of powders, pelletising of powders and fluids, coating with melts and polymers

toll manufacturing
Dursan

Dursan by SilcoTek

Innovative coating revolutionizes LC analysis

Stainless steel components with the performance of PEEK - inert, robust and cost-effective

HPLC accessories
Loading...

Most read news

More news from our other portals

See the theme worlds for related content

Topic World Battery Technology

The topic world Battery Technology combines relevant knowledge in a unique way. Here you will find everything about suppliers and their products, webinars, white papers, catalogs and brochures.

35+ products
150+ companies
40+ whitepaper
25+ brochures
View topic world
Topic World Battery Technology

Topic World Battery Technology

The topic world Battery Technology combines relevant knowledge in a unique way. Here you will find everything about suppliers and their products, webinars, white papers, catalogs and brochures.

35+ products
150+ companies
40+ whitepaper
25+ brochures